应用化学 ›› 2010, Vol. 27 ›› Issue (11): 1306-1312.DOI: 10.3724/SP.J.1095.2010.00026

• 研究论文 • 上一篇    下一篇

交联聚苯乙烯-丁二烯-苯乙烯双极膜的制备及其在电合成环氧丁二酸中的应用

黄雪红*,柯盛波,冀敏   

  1. (福建师范大学化学与材料学院,高分子材料重点实验室 福州 350007)
  • 收稿日期:2010-01-11 修回日期:2010-04-12 出版日期:2010-11-10 发布日期:2010-11-10
  • 通讯作者: 黄雪红,女,研究员; E-mail:xhhuang64@163.com; 研究方向:功能高分子
  • 基金资助:
    福建省科技厅福建省自然科学基金 (2009J05024)福建省高分子材料重点实验室开放基金(200802)福建师范大学本科生课外科技计划(BKL2009-049)资助项目

Preparation of Cross-linking Styrene-butadiene-styrene Triblock Copolymer Hybrid Bipolar Membrane and Its Application in Electro-generation of Trans-2,3-oxiranedicarboxylic Acid

HUANG Xue-Hong*, KE Sheng-Bo, JI Min   

  1. (College of Chemistry and Materials Science,Key Laboratory of Polymer
    Science,Fujian Normal University,Fuzhou 350007)
  • Received:2010-01-11 Revised:2010-04-12 Published:2010-11-10 Online:2010-11-10

摘要:

以聚苯乙烯-丁二烯-苯乙烯(SBS)嵌段共聚物作为基膜材料,采用自由基接枝聚合反应,在SBS主链上引入丙烯酸(AA)、苯乙烯磺酸和γ-甲基丙烯酰氧基丙基三甲氧基硅烷(KH570)链段作为阳离子交换膜;引入丙烯酸二甲基胺基乙酯和KH570链段作阴离子交换膜,阴、阳离子交换膜经KH570结构中三甲氧基硅烷基团的水解缩合,得到含硅氧交联网的SBS接枝离子交换膜,用流延法制备了SBS双极膜。 测得SBS阴膜和阳膜的吸水率分别为63.9%和72.8%,SBS阴膜和阳膜的离子交换容量分别为1.51和2.71 mmol/g。 将SBS双极膜作为阴阳两室隔膜,采用钨酸钠/过钨酸钠体系由阴极间接电氧化合成了环氧丁二酸。 结果表明,以石墨为阴、阳电极,电流密度为2.0×10-2 A/cm2、50 ℃反应4 h,环氧丁二酸的产率为53.0%,电流效率为40.8%。

关键词: SBS杂化双极膜, 间接电氧化, 钨酸钠/过钨酸钠, 环氧丁二酸

Abstract:

The crosslinking SBS hybrid bipolar membrane(SBS BPM) was prepared by free radical reaction of SBS(styrene-butadiene-styrene triblock copolymer) with acrylic acid(AA), sulfonic styrene(StSO3H) and γ-methacryloxypropyltrimethoxysilane(KH-570) as the anode membrane, and reaction of SBS with dimethyl amino ethyl methacrylate(DMAEMA) and KH-570 as the cathode membrane. Cross-linking reaction was carried out through sol-gel reaction of trimethoxysilane group. SBS BPM exhibited high temperature tolerance(thermal degradation temperature in N2, Td was up to 186.5 ℃). The ion exchange capacities(IECs) of the anode and cathode membranes were 1.51 and 2.71 mmol/g, respectively. SBS hybrid bipolar membranes were used as the separator in the electrolysis cell, then using tungstate/pertungstate as the media to indirect electrooxidate maleic acid to prepare trans2,3-oxiranedicarboxylic acid in the cathode chamber. Graphite was used as the anode and cathode electrode. At 50 ℃ and when the current density was 2.0×10-2 A/cm2 for 4 h, the yield and average current efficiency of trans2,3-oxiranedicarboxylic acid were 53.0% and 40.8%, respectively.

Key words: SBS hybrid bipolar membrane, indirect electrooxidate, tungstate /pertungstate, trans-oxiranedicarboxylic acid

中图分类号: