应用化学 ›› 2017, Vol. 34 ›› Issue (8): 877-884.DOI: 10.11944/j.issn.1000-0518.2017.08.160398

• 研究论文 • 上一篇    下一篇

阳离子型可聚合咪唑类离子液体-丙烯酰胺共聚物的制备及其对盐酸腐蚀碳钢缓蚀行为

丁红霞,武英,刘正平()   

  1. 北京师范大学化学学院,环境友好与功能高分子材料北京师范大学重点实验室; 能量存储与转化北京市重点实验室 北京 100875
  • 收稿日期:2016-09-30 接受日期:2017-06-07 出版日期:2017-07-25 发布日期:2017-07-26
  • 通讯作者: 刘正平
  • 基金资助:
    长江学者与创新团队发展计划及能量转换与存储材料北京市重点实验室开放基金资助

Preparation of Cationic Polymerizable Imdazolium Ionic Liquid-Acrylamide Copolymers and Their Inhibition Behaviors for Carbon Steel Corrosion in Hydrochloric Acid

DING Hongxia,WU Ying,LIU Zhengping()   

  1. BNU Key Lab of Environmentally Friendly and Functional Polymer Materials; Beijing Key Laboratory of Energy Convers & Storage Materials,College of Chemistry,Beijing Normal University,Beijing 100875,China
  • Received:2016-09-30 Accepted:2017-06-07 Published:2017-07-25 Online:2017-07-26
  • Contact: LIU Zhengping
  • Supported by:
    Supported by the Program for Changjiang Scholars and Innovative Research Team in University and the Open Foundation of Beijing Key Laboratory of Materials for Energy Conversion and Storage

摘要:

利用阳离子型可聚合离子液体1-丙烯酰氧乙基-3-甲基咪唑四氟硼酸盐与丙烯酰胺的反相微乳液共聚合,制备了阳离子型咪唑类离子液体-丙烯酰胺共聚物缓蚀剂,并探讨了其缓蚀性能。 研究了不同阳离子度、不同浓度聚合物溶液的缓蚀性能以及吸附时间对盐酸腐蚀碳钢速率的影响,并初步讨论了缓蚀机理。 研究表明,该种阳离子型缓蚀剂的缓蚀效率可达90%以上;缓蚀剂的缓蚀能力不仅取决于缓蚀剂的阳离子度,还取决于该种缓蚀剂的相对分子质量;缓蚀效率并非简单地随聚合物浓度的增加而提高,当聚合物溶液的浓度过高时,反而会使缓蚀效率下降;随吸附时间的延长,碳钢的腐蚀速率逐渐降低,约40 h后基本保持不变;加入缓蚀剂有效抑制了酸对铁的腐蚀,随缓蚀效率的提高,碳钢表面的粗糙程度明显降低,孔洞结构减少。

Key words: cationic polymerizable imdazolium ionic liquid, ionic liquid-acrylamide copolymer, cationic degree, corrosion inhibitor, corrosion mitigation mechanism